Aug 25, 2025 Fág nóta

Sonraíochtaí Píobán Druileála API 5DP

Réimse Píobáin Druileála API 5DP

Raon na méideanna: 2 3/8 "go {5 1/2"
Raon tiús: 6.5mm go 12.7mm
Fad: R1, R2, R3

 

Méide OD

Ainmniúil
Ualach

Ríomh an meáchan

Grád

Tiús

Foirm tiubhaithe (féach nóta)

i.

mm

LB/FT

kg/m

i.

mm

2 3/8

60.3

6.65

6.26

9.32

E,X,G,S

0.280

7.11

AE

2 7/8

73.0

10.4

9.72

14.48

E,X,G,S

0.362

9.19

AE, iu

3 1/2

88.9

9.50

8.81

13.12

E

0.254

6.45

AE, iu

3 1/2

88.9

13.30

12.31

18.34

E,X,G,S

0.368

9.35

AE, iu

3 1/2

88.9

15.50

14.63

21.79

E

0.449

11.40

AE, iu

3 1/2

88.9

15.50

14.63

21.79

X,G,S

0.449

11.40

AE, IEU

4

101.6

14.00

12.93

19.26

E,X,G,S

0.330

8.38

AE, iu

4 1/2

114.3

13.75

12.24

18.23

E

0.271

6.88

AE, iu

4 1/2

114.3

16.60

14.98

22.31

E,X,G,S

0.337

8.56

AE, IEU

4 1/2

114.3

20.00

18.69

27.84

E,X,G,S

0.430

10.92

AE, IEU

5

127.0

16.25

14.87

22.15

X,G,S

0.296

7.52

Ie

5

127.0

19.50

17.93

26.71

E

0.362

9.19

Ieu

5

127.0

19.50

17.93

26.71

X,G,S

0.362

9.19

AE, IEU

5

127.0

25.60

24.03

35.79

E

0.500

12.70

Ieu

5

127.0

25.60

24.03

35.79

X,G,S

0.500

12.70

AE, IEU

5 1/2

139.7

21.90

19.81

29.51

E,X,G,S

0.361

9.17

Ieu

5 1/2

139.7

24.70

22.54

33.57

E,X,G,S

0.415

10.54

Ieu

 

API 5DP drill pipe 

Glaoigh Linn

whatsapp

Fón

R-phost

Fiosrúchán