May 16, 2024 Fág nóta

Píobán Cruach Carbóin ERW

OD (Trastomhas Amach): 21.3-660mm
WT (Tiús an Bhalla): 1.0-20mm nó sch5, sch10, sch40, sch80, st, xs
Caighdeán:
le haghaidh píopa erw
ASTM A53 B% 2c A106% 2c ASTM A178% 2c ASTM A252
API 5L X42/46/52/56/60/70
ASTM A500, ASTM A513
GA 10204/10217 S235JR, S275JR, S355, S355JR, S355J2H
le haghaidh píopa efw
píobán efw cruach carbóin: ASTM A671, ASTM A672
píopa efw cruach cóimhiotail: ASTM A691
Cumhdach
Cumhdach 3PE
Cumhdach 3PP
Cumhdach FBE
Cumhdach Eapocsa
Péinteáil Speisialta

ERW Carbon Steel Pipe

Caoinfhulaingt Lasmuigh Trastomhas

Caighdeán Trastomhas Amach Caoinfhulaingt Deireadh Píob Caoinfhulaingt Comhlacht Píob
API 5L

219.1-273.1

+1.6mm, -0.4mm ±0.75%
274.0-320 +2.4mm, -0.8mm ±0.75%
323.9-457 +2.4mm, -0.8mm ±0.75%
508 +2.4mm, -0.8mm ±0.75%
559-610 +2.4mm, -0.8mm ±0.75%

Caoinfhulaingt Tiús Balla

Caighdeán Grád Trastomhas Amach Tiús bhalla
API 5L A 219.1-457 +15%, -12.5%
B 508-610 +17.5%, -12.5%
X42-X80 508-610 +19.5%, -8%

Anailís Cheimiceach agus Airíonna Meicniúla

Caighdeán Aicme Grád Anailís Cheimiceach(%) Airíonna Meicniúla(nóiméad)(Mpa)
C MNGenericName P S Neart Teanntachta Neart Toradh
API 5L PSL1 B 0.26 1.20 0.030 0.030 414 241
X42 0.26 1.30 0.030 0.030 414 290
X46 0.26 1.40 0.030 0.030 434 317
X52 0.26 1.40 0.030 0.030 455 359
X56 0.26 1.40 0.030 0.030 490 386
X60 0.26 1.40 0.030 0.030 517 414
X65 0.26 1.45 0.030 0.030 531 448
X70 0.26 1.65 0.030 0.030 565 483
PSL2Name B 0.22 1.20 0.025 0.015 414 241
X42 0.22 1.30 0.025 0.015 414 290
X46 0.22 1.40 0.025 0.015 434 317
X52 0.22 1.40 0.025 0.015 455 359
X56 0.22 1.40 0.025 0.015 490 386
X60 0.22 1.40 0.025 0.015 517 414
X65 0.22 1.45 0.025 0.015 531 448
X70 0.22 1.65 0.025 0.015 565 483
X80 0.22 1.85 0.025 0.015 621 552